PROCESS FOR TREATING ALUMINUM SURFACES

1419597 Sealing anodized A1 or alloys HENKEL & CIE GmbH 9 March 1973 [10 March 1972] 11465/73 Heading C7B Al or alloys thereof are anodized then sealed in an aqueous solution (pH 5-6.5) containing one or more water soluble phosphonic acids or water soluble salts thereof which form a complex with...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GEISLER, ROLAND, GERMSCHEID, HANS G, FRIEDEMANN, WOLFGANG
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GEISLER, ROLAND
GERMSCHEID, HANS G
FRIEDEMANN, WOLFGANG
description 1419597 Sealing anodized A1 or alloys HENKEL & CIE GmbH 9 March 1973 [10 March 1972] 11465/73 Heading C7B Al or alloys thereof are anodized then sealed in an aqueous solution (pH 5-6.5) containing one or more water soluble phosphonic acids or water soluble salts thereof which form a complex with a divalent metal, and calcium ions, the molar concentration of calcium ions to phosphonic acid being at least 2:1, and the solution temp 90‹C to boiling. The metal is first degreased with alkali then etched. The calcium ions may be supplied by CaCl 2 or Ca (NO 3 ) 2 . The solution may also contain 0.1-5.0 g/l dextrin. Examples of phosphonic acids include 1-hydroxypropane-, 1 diphosphonic acid, 1-amino ethane-, 1 diphosphonic acid, and aminotrimethylene phosphonic acid. The Na, K, ammonium or alkanolamine salts may be used.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CA1005788A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CA1005788A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CA1005788A3</originalsourceid><addsrcrecordid>eNrjZFALCPJ3dg0OVnDzD1IICXJ1DPH0c1dw9An19fQL9VUIDg1ycwTK8zCwpiXmFKfyQmluBnk31xBnD93Ugvz41OKCxOTUvNSSeGdHQwMDU3MLC0djwioASjsi0Q</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PROCESS FOR TREATING ALUMINUM SURFACES</title><source>esp@cenet</source><creator>GEISLER, ROLAND ; GERMSCHEID, HANS G ; FRIEDEMANN, WOLFGANG</creator><creatorcontrib>GEISLER, ROLAND ; GERMSCHEID, HANS G ; FRIEDEMANN, WOLFGANG</creatorcontrib><description>1419597 Sealing anodized A1 or alloys HENKEL &amp; CIE GmbH 9 March 1973 [10 March 1972] 11465/73 Heading C7B Al or alloys thereof are anodized then sealed in an aqueous solution (pH 5-6.5) containing one or more water soluble phosphonic acids or water soluble salts thereof which form a complex with a divalent metal, and calcium ions, the molar concentration of calcium ions to phosphonic acid being at least 2:1, and the solution temp 90‹C to boiling. The metal is first degreased with alkali then etched. The calcium ions may be supplied by CaCl 2 or Ca (NO 3 ) 2 . The solution may also contain 0.1-5.0 g/l dextrin. Examples of phosphonic acids include 1-hydroxypropane-, 1 diphosphonic acid, 1-amino ethane-, 1 diphosphonic acid, and aminotrimethylene phosphonic acid. The Na, K, ammonium or alkanolamine salts may be used.</description><language>eng</language><subject>APPARATUS THEREFOR ; CHEMISTRY ; ELECTROFORMING ; ELECTROLYTIC OR ELECTROPHORETIC PROCESSES ; METALLURGY ; PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><creationdate>1977</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19770222&amp;DB=EPODOC&amp;CC=CA&amp;NR=1005788A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19770222&amp;DB=EPODOC&amp;CC=CA&amp;NR=1005788A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GEISLER, ROLAND</creatorcontrib><creatorcontrib>GERMSCHEID, HANS G</creatorcontrib><creatorcontrib>FRIEDEMANN, WOLFGANG</creatorcontrib><title>PROCESS FOR TREATING ALUMINUM SURFACES</title><description>1419597 Sealing anodized A1 or alloys HENKEL &amp; CIE GmbH 9 March 1973 [10 March 1972] 11465/73 Heading C7B Al or alloys thereof are anodized then sealed in an aqueous solution (pH 5-6.5) containing one or more water soluble phosphonic acids or water soluble salts thereof which form a complex with a divalent metal, and calcium ions, the molar concentration of calcium ions to phosphonic acid being at least 2:1, and the solution temp 90‹C to boiling. The metal is first degreased with alkali then etched. The calcium ions may be supplied by CaCl 2 or Ca (NO 3 ) 2 . The solution may also contain 0.1-5.0 g/l dextrin. Examples of phosphonic acids include 1-hydroxypropane-, 1 diphosphonic acid, 1-amino ethane-, 1 diphosphonic acid, and aminotrimethylene phosphonic acid. The Na, K, ammonium or alkanolamine salts may be used.</description><subject>APPARATUS THEREFOR</subject><subject>CHEMISTRY</subject><subject>ELECTROFORMING</subject><subject>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</subject><subject>METALLURGY</subject><subject>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1977</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFALCPJ3dg0OVnDzD1IICXJ1DPH0c1dw9An19fQL9VUIDg1ycwTK8zCwpiXmFKfyQmluBnk31xBnD93Ugvz41OKCxOTUvNSSeGdHQwMDU3MLC0djwioASjsi0Q</recordid><startdate>19770222</startdate><enddate>19770222</enddate><creator>GEISLER, ROLAND</creator><creator>GERMSCHEID, HANS G</creator><creator>FRIEDEMANN, WOLFGANG</creator><scope>EVB</scope></search><sort><creationdate>19770222</creationdate><title>PROCESS FOR TREATING ALUMINUM SURFACES</title><author>GEISLER, ROLAND ; GERMSCHEID, HANS G ; FRIEDEMANN, WOLFGANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CA1005788A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1977</creationdate><topic>APPARATUS THEREFOR</topic><topic>CHEMISTRY</topic><topic>ELECTROFORMING</topic><topic>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</topic><topic>METALLURGY</topic><topic>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</topic><toplevel>online_resources</toplevel><creatorcontrib>GEISLER, ROLAND</creatorcontrib><creatorcontrib>GERMSCHEID, HANS G</creatorcontrib><creatorcontrib>FRIEDEMANN, WOLFGANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GEISLER, ROLAND</au><au>GERMSCHEID, HANS G</au><au>FRIEDEMANN, WOLFGANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PROCESS FOR TREATING ALUMINUM SURFACES</title><date>1977-02-22</date><risdate>1977</risdate><abstract>1419597 Sealing anodized A1 or alloys HENKEL &amp; CIE GmbH 9 March 1973 [10 March 1972] 11465/73 Heading C7B Al or alloys thereof are anodized then sealed in an aqueous solution (pH 5-6.5) containing one or more water soluble phosphonic acids or water soluble salts thereof which form a complex with a divalent metal, and calcium ions, the molar concentration of calcium ions to phosphonic acid being at least 2:1, and the solution temp 90‹C to boiling. The metal is first degreased with alkali then etched. The calcium ions may be supplied by CaCl 2 or Ca (NO 3 ) 2 . The solution may also contain 0.1-5.0 g/l dextrin. Examples of phosphonic acids include 1-hydroxypropane-, 1 diphosphonic acid, 1-amino ethane-, 1 diphosphonic acid, and aminotrimethylene phosphonic acid. The Na, K, ammonium or alkanolamine salts may be used.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CA1005788A
source esp@cenet
subjects APPARATUS THEREFOR
CHEMISTRY
ELECTROFORMING
ELECTROLYTIC OR ELECTROPHORETIC PROCESSES
METALLURGY
PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS
title PROCESS FOR TREATING ALUMINUM SURFACES
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T04%3A21%3A56IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GEISLER,%20ROLAND&rft.date=1977-02-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECA1005788A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true