LEAD ALLOY
The alloy is used for making storage battery grids. It has high corrosion resistance and improved flowability. The lead alloy has the following composition in mass percentage: antimony 0.8-3.0, arsenic 0.1-0.3, tin 0.1-0.3, copper 0.03-0.08, selenium-0.01 - 0.06, bismuth 0.03-0.03, sodium 0.005-0.03...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The alloy is used for making storage battery grids. It has high corrosion resistance and improved flowability. The lead alloy has the following composition in mass percentage: antimony 0.8-3.0, arsenic 0.1-0.3, tin 0.1-0.3, copper 0.03-0.08, selenium-0.01 - 0.06, bismuth 0.03-0.03, sodium 0.005-0.03 and the rest lead. |
---|