Refractory and nozzle for casting
The present invention provides for long-term prevention of hydration (slaking) of CaO during a production stage, during storage, and during an operation stage in a refractory comprising a CaO component. That is, this refractory comprises refractory particles including a CaO component and refractory...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The present invention provides for long-term prevention of hydration (slaking) of CaO during a production stage, during storage, and during an operation stage in a refractory comprising a CaO component. That is, this refractory comprises refractory particles including a CaO component and refractory particles including an MgO component, where a chemical component after heating in a 1,000°C non-oxidizing atmosphere contains 0.1-5.0 mass% in total of one or more species of metal oxide selected from B |
---|