Delayed, swellable particles for prevention of fluid migration through damaged cement sheaths
A method includes providing a cementing composition that includes an aqueous fluid, a cementitious particulate, and a copolymer particulate which includes a monofunctional monomer, a water degradable first crosslinker, and a second crosslinker. The method further includes placing the cementing compo...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method includes providing a cementing composition that includes an aqueous fluid, a cementitious particulate, and a copolymer particulate which includes a monofunctional monomer, a water degradable first crosslinker, and a second crosslinker. The method further includes placing the cementing composition in a subterranean formation so as to form a set cement sheath and swelling the copolymer particulate in response to a void created in the set cement sheath. The copolymer particulate allows the cementing composition to set to form the cement sheath before substantial swelling of the copolymer particulate occurs. |
---|