Method for producing silver nanofilaments
A method of producing silver nanofilaments that is relatively fast and may be carried out at normal room temperatures (e.g., from about 10°C to about 25°C). The method of producing silver nanofilaments includes the steps of adding a solid silver salt to liquid ether to form a mixture, adding a liqui...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method of producing silver nanofilaments that is relatively fast and may be carried out at normal room temperatures (e.g., from about 10°C to about 25°C). The method of producing silver nanofilaments includes the steps of adding a solid silver salt to liquid ether to form a mixture, adding a liquid fatty acid to the mixture, adding a reducing agent to the mixture, allowing the ingredients to react, and recovering silver nanofilaments. |
---|