VERFAHREN ZUR EINSTELLUNG VON SUPERPLASTISCHEN EIGENSCHAFTEN IN MAGNESIUMLEGIERUNGEN
Production of magnesium alloys having a superplastic structure comprises heating a magnesium-based alloy to 250-600 degrees C; deforming to a semi-finished product at 250-450 degrees C; and rapidly cooling at a speed of more than 300 degrees C/minute.