VERFAHREN ZUR HERSTELLUNG VON ELASTOMEREN ETHYLENCOPOLYMERISATEN MIT HOHER ZUGFESTIGKEIT DES ROHPRODUKTES

Elastomeric copolymers of ethylene including: (a) 60-90% in moles of ethylene; (b) 1-30% in moles of an alpha -olefin CH2=CHR, where R is an alkyl radical having from 2 to 6 carbon atoms; (c) 0-20% in moles of propylene; the sum of percentages (a), (b) and (c) being equal to 100, and the crude produ...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BANZI, VIVIANO, LOBERTI, GIANNI, CALDARI, SILVIA
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Elastomeric copolymers of ethylene including: (a) 60-90% in moles of ethylene; (b) 1-30% in moles of an alpha -olefin CH2=CHR, where R is an alkyl radical having from 2 to 6 carbon atoms; (c) 0-20% in moles of propylene; the sum of percentages (a), (b) and (c) being equal to 100, and the crude product having an ultimate tensile stress of between 10 and 200 kg/cm .