VERFAHREN UND VORRICHTUNG ZUR MAHLUNG VON FASERSTOFFEN

To beat wood and other fiber materials, the material is passed between two beating surfaces, where the speed difference between them is between 5 m/second and 12 m/second or zero. The material is fed as a web (6) between two rotating rollers (2,3) in a beater (1), to be spread evenly over their beat...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: GABL HELMUTH. DR
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To beat wood and other fiber materials, the material is passed between two beating surfaces, where the speed difference between them is between 5 m/second and 12 m/second or zero. The material is fed as a web (6) between two rotating rollers (2,3) in a beater (1), to be spread evenly over their beating surfaces. The rollers are rotated by motors (4,5).