Fluorine-Labeling as a Diagnostic for Thiol-Ligand and Gold Nanocluster Self-Assembly
An omega-fluorine-labeled oxyethylene thiol ligand, F(CH2CH2O)2CH2CH2SH, was synthesized, characterized and incorporated into mixed self-assembled monolayers with CH3(OCH2CH2)3SH onto a planar gold substrate and onto 2 nm gold nanoclusters. The fluorine-labeled nanocluster was selfassembled onto gol...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Report |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | An omega-fluorine-labeled oxyethylene thiol ligand, F(CH2CH2O)2CH2CH2SH, was synthesized, characterized and incorporated into mixed self-assembled monolayers with CH3(OCH2CH2)3SH onto a planar gold substrate and onto 2 nm gold nanoclusters. The fluorine-labeled nanocluster was selfassembled onto gold substrates using alkane dithiol (HS(CH2)nSH; n = 5, 8, 11) and oxyethylene dithiol (HS(CH2CH2O)nCH2CH2SH; n = 1, 2, 3) linking agents with equivalent chain lengths for comparative purposes. X-ray photoelectron spectroscopy (XPS) was used to track the fluorine-label in the self-assembly operations and to evaluate the effectiveness of the dithiols. For adequate XPS sensitivity at least 10% of the monolayer-forming molecules should be functionalized with this fluorinelabel. In the comparative self-assembly of the fluorine-labeled gold nanoclusters in chloroform solution, the alkane dithiols were observed to be the more effective linking agents. This effectiveness correlates with the XPS analysis of alkane dithiols self-assembling onto the gold substrates with a higher packing density and with a larger fraction of molecules having one thiol group as opposed to two bonded to the gold surface. The oxyethylene dithiols self-assemble with a smaller packing density and a smaller fraction of molecules with an unbonded thiol group available for self-assembly.
Published in Analyst, v134 p1790-1801, 2009. |
---|