Failure Analysis of a Sodium Heat Pipe with Integral Lithium Fluoride Thermal Energy Storage

A sodium, 321 stainless steel heat pipe with three filled Nb-1Zr tubes for thermal energy storage with 304 S.S. screen for wicking was thermal cycled to failure and then an analysis was performed to examine the failure. It was concluded that insufficient weld depth between an end cap and tube body p...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Jacobson,Dean L, Soundararajan,P
Format: Report
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A sodium, 321 stainless steel heat pipe with three filled Nb-1Zr tubes for thermal energy storage with 304 S.S. screen for wicking was thermal cycled to failure and then an analysis was performed to examine the failure. It was concluded that insufficient weld depth between an end cap and tube body permitted the propagation of a crack through a possible combination of thermal/corrosion failure, creep rupture of the end cap. A number of possible scenarios for the process following a leak are discussed.