Properties of DEXSIL 300 Rubbers
The physical and elastomeric properties of several DEXSIL 300 (10-SiB-3) samples were investigated. Modulus-temperature studies were used to determine the glass transition temperature, the melting temperature, and the oxidative crosslinking temperature. Stress relaxation in air at elevated temperatu...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Report |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The physical and elastomeric properties of several DEXSIL 300 (10-SiB-3) samples were investigated. Modulus-temperature studies were used to determine the glass transition temperature, the melting temperature, and the oxidative crosslinking temperature. Stress relaxation in air at elevated temperatures was used to compare the oxidative stability of the various formulations. (Author) |
---|