Physical Properties of Boards Manufactured with Hygrothermally Treated Tepa (Laureliopsis Philippiana Looser) Particles
Three layer particleboards were manufactured using hygrothermally treated and untreated Laureliopsis philippiana (tepa) particles with urea-formaldehyde (UF) resin. Hygrothermal treatment consisted of autoclaving particles at 150 °C for 90 min (430 kPa) in a steam saturated atmosphere. Density, mois...
Gespeichert in:
Veröffentlicht in: | Drvna industrija 2016-09, Vol.67 (3), p.263-270 |
---|---|
Hauptverfasser: | , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Three layer particleboards were manufactured using hygrothermally treated and untreated Laureliopsis philippiana (tepa) particles with urea-formaldehyde (UF) resin. Hygrothermal treatment consisted of autoclaving particles at 150 °C for 90 min (430 kPa) in a steam saturated atmosphere. Density, moisture content, swelling and water absorption were determined. Equilibrium moisture, dimensional variation in length and thickness, as well as length and thickness coefficients per every 1 % change in board equilibrium moisture were also determined after acclimatization at different relative air humidity conditions (20 °C; 40, 50, 60, 70, 80 and 90 % RAH). There were significant differences between particleboards made from control and treated particles. Boards manufactured with treated particles showed a reduction in moisture content, swelling and water absorption. Dimensional stability analysis in response to relative air humidity (RAH) showed that the hygrothermal treatment causes a reduction in equilibrium moisture, a decrease in length and thickness dimensional variation, likewise a reduction in length and thickness swelling coefficients. |
---|---|