Micro Push-Out Bond Strength of Resin Composite to Dentin in Primary Dentition Using Three Universal Adhesives with Different pH: An In Vitro Study

To evaluate the bond strength of different universal adhesives on deciduous tooth dentineand their relationship with the composition and potential of hydrogen (pH). Methods: An in vitromicro push-out test on 150 samples (n = 50) per group per adhesive, namely, Adhese Universal(ADH; Ivoclar Vivadent)...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied sciences 2021-07, Vol.11 (14), p.6349
Hauptverfasser: Del Río Carrillo, Regina María, Molinero-Mourelle, Pedro, Vera, Vicente, Romero Villaba, Pablo, Casañas, Elizabeth, Fonseca, Manrique, Vera-Gonzalez, Vicente, Mourelle-Martinez, María Rosa
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To evaluate the bond strength of different universal adhesives on deciduous tooth dentineand their relationship with the composition and potential of hydrogen (pH). Methods: An in vitromicro push-out test on 150 samples (n = 50) per group per adhesive, namely, Adhese Universal(ADH; Ivoclar Vivadent), Futurabond U (FUT; Voco GmbH) (Test), and Scotchbond Universal withpre-conditioning (SCO; 3M) (Control), to record bond strength (BS) and type of adhesive failure.Results: The results of the different adhesives (megapascals (MPa)) varied, showing no statisticalsignificance. The corresponding averages are in MPa: ADH, 13.66 2.81; FUT, 14.48 2.88; SCO,14.98 3.96. Additionally, the frequency of type of failure was as follows: mixed (60.7%), adhesive(27.3%), and cohesive (12%). Conclusions: SCO, with a pH of 2.7, showed greater resistance tofracture, while FUT, with a pH of 2.3 and no pre-conditioning, approached the same values, being aone-step adhesive. No relationship was found between failure and type of adhesive.
ISSN:2076-3417
2076-3417
DOI:10.3390/app11146349