Mechanical properties of hot-pressed Al-4.5 wt. % Cu/WC composite

In this study, the elemental powders of aluminum and copper were initially subjected to mechanical alloying using an attrition ball mill under argon atmosphere to produce an Al-4.5 wt% Cu powder alloy. The WC nanoparticles were then added to the powder alloy and milled in a planetary ball mill to ex...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of ultrafine grained and nanostructured materials 2014-12, Vol.47 (2), p.63-70
Hauptverfasser: Samaneh Bernoosi, Rasoul Azari Khosroshahi, Reza Taherzadeh Mousavian
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In this study, the elemental powders of aluminum and copper were initially subjected to mechanical alloying using an attrition ball mill under argon atmosphere to produce an Al-4.5 wt% Cu powder alloy. The WC nanoparticles were then added to the powder alloy and milled in a planetary ball mill to explore the role of the WC nanoparticles on the mechanical properties of the fabricated composite powder. The experimental results revealed that a solid solution of Al-Cu could be formed after MA and a good dispersion of the WC nanoparticles in the aluminum matrix was obtained as characterized using X-ray diffraction and scanning electron microscopy, respectively. The results of hardness and compression tests of the hot pressed composites indicated that the MA followed by the hot-press processes was successful to fabricate an alloy and a metal matrix composite with considerable mechanical properties. However, a decreasing trend in the hardness and strength of the composites with the WC contents of more than 5wt% was observed. The maximum values of 260 HV and 575 MPa were obtained for a composite containing 5 wt% of nano ceramic particles.