Extraction of Lithium from Spent Lithium-ion Batteries (LIBs) using Cation Exchange Resin

Considering the lithium (Li) supply crisis and the regulations around recycling, sustainable extraction of Li from spent lithium-ion batteries (LiBs) is critical. Recently, recovery of Li from spent LiBs by water leaching has been investigated, and a high leaching selectivity towards Li is reported...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:E3S web of conferences 2024, Vol.543, p.2010
Hauptverfasser: Farooq, Hammad, Buzaljko, Lejla, Bandyopadhyay, Sulalit
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Considering the lithium (Li) supply crisis and the regulations around recycling, sustainable extraction of Li from spent lithium-ion batteries (LiBs) is critical. Recently, recovery of Li from spent LiBs by water leaching has been investigated, and a high leaching selectivity towards Li is reported by fine-tuning the pH among other factors leading to the introduction of Na + ions, which complicates selective Li recovery. Further, the low Li concentration makes the downstream precipitation challenging without an intermediate energy-intensive evaporative step. Herein, we employ Amberlite-H + , a commercially available cation exchange resin to investigate its suitability in the extraction of Li from water leachates of black mass. The water leachate containing 135 mg/L Li was prepared at optimized conditions of 25 °C, S/L (black mass/water) of 20 g/L, and a pH of 10. The extraction of Li from this water leachate by Amberlite-H + was studied to optimize the reaction time, and various S/L ratios of Amberlite-H + to leachate were investigated. The kinetic experiments showed that the extraction of Li from the water leachate reaches equilibrium before 30 minutes. The effect of S/L ratios was investigated at the optimized reaction time and the results showed that at S/L (g/L) of 20, 40, and 60, the uptake capacity of Li (mgLi + /gresin) is 5.34, 3.06, and 2.15, respectively. The Li-loaded resins were washed with 100 mL of 1 M HCl to desorb Li, achieving 97 – 99 % desorption yield.
ISSN:2267-1242
2267-1242
DOI:10.1051/e3sconf/202454302010