Tear Strength Analysis of MDX4-4210 and A-2186 Silicones with Different Intrinsic Pigments Incorporated by Mechanical and Industrial Methods

Objective. The aim of this study was to evaluate the tear strength of MDX4-4210 and A-2186 silicones with different intrinsic pigments incorporated by mechanical and industrial methods, comparing nonaged and aged groups. Materials and Methods. Twenty-four groups were created according to the America...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:International journal of dentistry 2019, Vol.2019 (2019), p.1-7
Hauptverfasser: Lamartine de Moraes Melo Neto, Clovis, Pinheiro de Magalhães Bertoz, André, Micheline dos Santos, Daniela, Silva, Emily Vivianne Freitas da, Nobrega, Adhara Smith, Goiato, Marcelo Coelho, Sonego, Mariana Vilela
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Objective. The aim of this study was to evaluate the tear strength of MDX4-4210 and A-2186 silicones with different intrinsic pigments incorporated by mechanical and industrial methods, comparing nonaged and aged groups. Materials and Methods. Twenty-four groups were created according to the American Society for Testing and Materials D-624/type C, half nonaged and half aged (n = 10): bronze mechanical MDX4-4210, bronze industrial MDX4-4210, black mechanical MDX4-4210, black industrial MDX4-4210, pink mechanical MDX4-4210, pink industrial MDX4-4210, bronze mechanical A-2186, bronze industrial A-2186, black mechanical A-2186, black industrial A-2186, pink mechanical A-2186, and pink industrial A-2186. All specimens were submitted to tear strength analysis. Data were submitted to the ANOVA and Tukey test (p
ISSN:1687-8728
1687-8736
DOI:10.1155/2019/2573095