Mechanical and thermal characterization of a beet pulp-starch composite for building applications
This work shows the making of a new bio-based material for building insulation from sugar beet pulp and potato starch. The material is both lightweight and ecofriendly. The influence of starch/ sugar beet pulp ratio (S/BP) is studied. Four binder mass dosages are considered, 10, 20, 30 and 40% (rela...
Gespeichert in:
Veröffentlicht in: | E3S web of conferences 2019-01, Vol.85, p.8005 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | This work shows the making of a new bio-based material for building insulation from sugar beet pulp and potato starch. The material is both lightweight and ecofriendly. The influence of starch/ sugar beet pulp ratio (S/BP) is studied. Four binder mass dosages are considered, 10, 20, 30 and 40% (relative to the beet pulp). Samples are characterized in terms of absolute and bulk density, compressive and flexural strength, as well as thermal properties (thermal conductivity and thermal inertia). The compressive strength increases linearly with the S/BP mass ratio to reach 0.52 MPa and the compressive strain is 30%. The thermal conductivity is to around 0.070 W/m. K. The results obtained shows that increasing starch amount tends to decrease composite porosity but increases thermal conductivity and mechanical properties. Depending on the starch content, beet pulp composites have a good thermal and can be used as building materials. |
---|---|
ISSN: | 2267-1242 2555-0403 2267-1242 |
DOI: | 10.1051/e3sconf/20198508005 |