Wear Behavior of Bioactive Glass Coatings Deposited by Thermal Spraying

In this work, bioactive glass coatings were fabricated by plasma thermal spraying and oxyacetylene flame techniques from 2 different bioactive glass powders with 0 and 2% molar MgO. The metal substrates used were Ti6Al4V alloy and AISI 316L steel. The tribological behavior of the coatings was evalua...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Revista FI-UPTC 2022-11, Vol.31 (62), p.e14778
Hauptverfasser: Monsalve-Arias, Mónica-Johanna, Higuera-Cobos, Oscar-Fabián, Ageorges, Helèn, Vargas-Galvis, Fabio, López-Gómez, María-Esperanza
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In this work, bioactive glass coatings were fabricated by plasma thermal spraying and oxyacetylene flame techniques from 2 different bioactive glass powders with 0 and 2% molar MgO. The metal substrates used were Ti6Al4V alloy and AISI 316L steel. The tribological behavior of the coatings was evaluated by the ball-on-disc method in the presence of simulated biological fluid (SBF), and the results were correlated with their mechanical behavior, obtaining values of hardness (between 4.84 and 5.18 GPa) and fracture toughness (between 5.25 and 6.62 MPa.m1/2). The results show that fracture toughness has a slightly higher effect than hardness on the wear behavior of the coatings under study.
ISSN:0121-1129
2357-5328
2357-5328
DOI:10.19053/01211129.v31.n62.2022.14778