The Enhancing Corrosion Inhibition for Low Carbon Steel by Adding Graphene Oxide- WO3 in Epoxy Resin Matrix

 In this research, polyanthranilic acid, graphene oxide, and tungsten oxide nanoparticles were prepared. In the next step, GO-10%WO3, nanocomposite was prepared by adding the 10% of the weight ratio of tungsten oxide. In another step, a solution of polyanthranilic acid was mixed with epoxy resin to...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Academic Science Journal 2024-10, Vol.2 (4)
1. Verfasser: WASAN ABDULFATAH HUSEEIN
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung: In this research, polyanthranilic acid, graphene oxide, and tungsten oxide nanoparticles were prepared. In the next step, GO-10%WO3, nanocomposite was prepared by adding the 10% of the weight ratio of tungsten oxide. In another step, a solution of polyanthranilic acid was mixed with epoxy resin to prepare the mother solution (Epoxy-PANA). In the last step, polymeric coatings (GO /Epoxy-PANA, GO-10%WO3/Epoxy-PANA) were prepared, in addition to (Epoxy-PANA). The prepared materials were characterized by FTIR, XRD, EDX and SEM. In the end, it’s use as anti-corrosion materials by coating it with low carbon steel. It was found that Inhibition efficiency increased by adding tungsten oxide nanoparticles to the coatings. On the other hand, the corrosion rate is reduced by adding tungsten. Moreover, it was found that adding the percentage10% of WO3 leads to affects the activation energy (Ea), enthalpy (∆H) and entropy (∆S), and this has been studied as well.