Evaluation of the bond strength of three soft lining materials to acrylic resin denture base

Aims : the aims of this study were to evaluate the effect of different surface treatments and different periods of water storage on tensile bond strength of three soft lining materials. Materials and me-thuds : Two hundred sixty four (264) specimens have been prepared. Surface treatments used for bo...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Al-Rafidain Dental Journal 2012, Vol.12 (1), p.57-65
Hauptverfasser: Kazanji, Mundhir N., al-Khidr, Asmaa A. Abd
Format: Artikel
Sprache:ara ; eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Aims : the aims of this study were to evaluate the effect of different surface treatments and different periods of water storage on tensile bond strength of three soft lining materials. Materials and me-thuds : Two hundred sixty four (264) specimens have been prepared. Surface treatments used for bonding Molloplast B liner included roughening acrylic surface with bur, and treatment with primo adhesive. For bonding Bony plus liner, roughening acrylic surface with bur, treatment with liner’s liquid and combination of both treatments have been evaluated. For GC Reline liner, roughening acrylic surface with bur has been evaluated. Before tensile bond testing of Molloplast-B liner’s specimens they were stored for(1 day or 1 month or 4 months), while Bony plus and GC Reline liners’ specimens were stored for(1 day or 1 week or 1 month) and then tested. Results: The results showed that roughening acrylic surface had an insignificant effect on (TBS) of GC Reline liner and Bony plus liner (although these materials showed cohesive failure). Bony plus liner’s liquid treatments had significant improvement in (TBS) of this liner. Different periods of water storage had insignificant effect on (TBS) of Molloplast-B liner and GC Reline liner, but (TBS) of Bony plus liner showed significant increasing after 1-month water storage. Conclusion: From the results of this study we can concluded that surface treatment to acrylic base improved tensile bond strength of soft lining material ,and the effect of water storage on bond strength differed with different types of soft lining materials. الأهداف : تهدف الدراسة إلى تحديد تأثير أنواع مختلفة من معالجات الأسطح و أوقات مختلفة من الخزن المائي على قوة الارتباط الثدي لثلاثة أنواع مختلقه من المبطنات الطرية للأطقم السنية. المواد و طرائق السل : تم استخدام 294 عينة لهذا البحث و المعالجات السطحية المستخدمة مع مادة ال (Molloplast-B) شملت تخشين السطح بالسنبلة و استخدام مادة ال (primo adhesive). بالنسبة لمادة (Bony plus) و قد تم تخشين السطح السنبلة فضلا عن استخدام ال (liner liquid). بالنسبة لمادة ال (G C Reline) حيث تم استخدام طريقة التخشين بالسنبلة فقط، قبل قياس قوة الارتباط الثدي كذلك تم خزن عينات البحث لمادة ال (molloplast B) لفترات مختلفة هي : (1 يوم وشهر و أربعة أشهر) بينما لمادة ال (GC Reline) j(Bony plus) كان الخزن للفترات(. يوم واحد و أسبوع وشهر واحد) قبل الفحص. النتائج : أظهرت النتائج أن تخشين سطح مادة الاكريل باستخدام السنبلة له تأثير معنوي على قوة الارتباط ألشدي لمادتي ال (Bony plus linerjGCReline). كذلك أظهرت مادة ال bony plus lin
ISSN:1812-1217
1998-0345
1998-0345
DOI:10.33899/rden.2012.42630