Synthesis of Chitosan/Zinc Oxide Nanoparticles Stabilized by Chitosan via Microwave Heating

Nowadays, zinc oxide (ZnO) has attracted attention in research and development because of its remarkable antibacterial properties. Chitosan/ZnO nanoparticles were successfully synthesized via microwave heating. The objectives of this work were to investigate the effect of stabilizer, power heating a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Bulletin of chemical reaction engineering & catalysis 2019-08, Vol.14 (2), p.450-458
Hauptverfasser: Ahmad Yusof, Nurul Amira, Mat Zain, Norashikin, Pauzi, Norlin
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Nowadays, zinc oxide (ZnO) has attracted attention in research and development because of its remarkable antibacterial properties. Chitosan/ZnO nanoparticles were successfully synthesized via microwave heating. The objectives of this work were to investigate the effect of stabilizer, power heating and time heating on size of chitosan/ZnO nanoparticles and to determine antibacterial activity against pathogenic bacteria, where chitosan was used as a stabilizing agent. Chitosan/ZnO nanoparticles were analyzed  by Fourier Transform Infra Red (FTIR), X-ray Diffraction (XRD), Field Emission Scanning Electron Microscopy (FESEM), and Zetasizer instrument. The power heating and time heating were varied from 400 to 800 Watt and 4 to 8 minutes, respectively. The presence of chitosan has role on preventing the nanoparticles from agglomeration by producing a milky solution of chitosan/ZnO nanoparticles without any suspensions. The increase of power  and time heating improved the size of nanoparticles. The peak in FTIR spectrum at around 427 cm-1 was confirmed the existence of the ZnO phase. XRD patterns showed that the chitosan/ZnO nanoparticles materials were pure phase with average crystalline size is 130 nm. FESEM revealed that chitosan/ZnO nanoparticles were uniformly distributed with the mean value of size is 70 nm and spherical shaped. Further impact of power and time heating on the size of the chitosan/ZnO nanoparticles can be shown by a nanoparticles size distribution with the average of 30 to 90 nm. The results showed that chitosan/ZnO nanoparticles have displayed an antibacterial inhibition zone against Gram-positive S. aureus and Gram-negative E. coli which 16.0 and 13.3 mm, respectively. Chitosan/ZnO nanoparticles were synthesized in this work presented have potential application to prevent bacterial infections. 
ISSN:1978-2993
1978-2993
DOI:10.9767/bcrec.14.2.3319.450-458