Study on Thermal Performance of Electric Heating System with Salt Hydrate-PCM Storage
An electric radiator combined with salt hydrate-phase change material (PCM) storage was developed to replace the existing scattered coal burning systems for clean heating applications. It was designed to have an average heat output of 400 W and a thermal storage efficiency of 65.6% for reducing the...
Gespeichert in:
Veröffentlicht in: | Energies (Basel) 2023-10, Vol.16 (20), p.7108 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | An electric radiator combined with salt hydrate-phase change material (PCM) storage was developed to replace the existing scattered coal burning systems for clean heating applications. It was designed to have an average heat output of 400 W and a thermal storage efficiency of 65.6% for reducing the electricity peak load. The thermal performance was investigated experimentally and numerically by using various radiator configurations and electric heating powers, as well as three PCMs with a melting point of 58 °C (PCMI 58), 78 °C (PCMI 78) and 90 °C (PCMI 90). It was found that the radiator combined with PCMI 78 had an average heat output of 412 W, and the PCMI 78 could be completely charged within 8 off-peak hours at an electric heating power of 1270 W, in the case of the radiator external dimension L × B × H of 796 × 106 × 656 mm and the L/B ratio of 7.5. The experiment results indicated that the average room temperature could be maintained at 20.0 °C at an outdoor temperature of 5.2 °C when applying the electric radiator developed. |
---|---|
ISSN: | 1996-1073 1996-1073 |
DOI: | 10.3390/en16207108 |