Influence of welding parameters and post-weld aging on tensile properties and fracture location of AA2139-T351 friction-stir-welded joints

Tensile properties and fracture location of AA2139-T351 friction stir welded joints are studied in the as-welded and post-weld aged condition. The experimental results show that when the joints are free of welding defects, they fail on the advancing side of the HAZ exhibiting a large amount of plast...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials research (São Carlos, São Paulo, Brazil) São Paulo, Brazil), 2013-09, Vol.16 (5), p.1106-1112
Hauptverfasser: Prisco, Umberto, Squillace, Antonino, Astarita, Antonello, Velotti, Carla
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Tensile properties and fracture location of AA2139-T351 friction stir welded joints are studied in the as-welded and post-weld aged condition. The experimental results show that when the joints are free of welding defects, they fail on the advancing side of the HAZ exhibiting a large amount of plastic deformation. When the revolutionary pitch exceeds a threshold value, some micro-defects are formed in the weld nugget due to insufficient heat input. In this case, the joints fail near the weld center, and the fracture occurs in a mixed mode, both ductile and brittle. However, being less ductile, post-weld aged joints are less defect-tolerant and, then, they fracture closer to the weld center, showing a reduced elongation at fracture and an UTS within the order of magnitude of the as-welded joints.
ISSN:1516-1439
1980-5373
1980-5373
DOI:10.1590/S1516-14392013005000099