Videographic Data for Pore Formation and Melt Pool Analysis of Laser Welded Al-Cu Joints using Synchrotron Radiation
The published data include video recordings of synchrotron radiation during a laser beam welding process in aluminium-copper joints. The recordings show the phase boundaries of the materials and are suitable for an analysis with regard to material mixing and pore formation. The experiments were cond...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Video |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The published data include video recordings of synchrotron radiation during a laser beam welding process in aluminium-copper joints. The recordings show the phase boundaries of the materials and are suitable for an analysis with regard to material mixing and pore formation. The experiments were conducted with the high energy beamline P07 (EH4) of Petra 3 at Deutsches Elektronen Synchrotron DESY in Hamburg, Germany. General parameters: Photon energy of synchrotron beam: 37,7 keV Scintillator material: CdWO4 Frame rate: 1000 Hz Specific parameters used for videos: HV185: Cu-ETP (top) to Al99.5 (bottom); wavelengths of laser beam source: 1030 nm; laser beam diameter: 117 µm; laser power: 1000 W; feed rate: 50 mm/s HV186: Cu-ETP (top) to Al99.5 (bottom); wavelengths of laser beam source: 1030 nm; laser beam diameter: 117 µm; laser power: 1500 W; feed rate: 100 mm/s HV192: Al99.5 (top) to CuSn6 (bottom); wavelengths of laser beam source: 1070 nm; laser beam diameter: 34 µm; laser power: 750 W; feed rate: 50 mm/s HV196: Cu-ETP (top) to Al99.5 (bottom); wavelengths of laser beam source: 1070 nm; laser beam diameter: 34 µm; laser power: 750 W; feed rate: 50 mm/s |
---|---|
DOI: | 10.5281/zenodo.6411748 |