Creasing severity and reverse-side cracking

Crease cracking can be detrimental to the functionality and appearance of paperboard-based pack-aging. The effect of creasing severity on the degree of reverse-side crease cracking (bead-side of the crease) of paperboard was investigated. Samples were creased with a range of rule and channel geometr...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Tappi journal 2020-05, Vol.19 (4), p.219-227
Hauptverfasser: PANEK, JOEL C., SMITH, SWAN D., COFFIN, DOUGLAS W.
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Crease cracking can be detrimental to the functionality and appearance of paperboard-based pack-aging. The effect of creasing severity on the degree of reverse-side crease cracking (bead-side of the crease) of paperboard was investigated. Samples were creased with a range of rule and channel geometries, and the cracking degree was quantified as the percent of cracked length relative to the total length of the crease. The cracking degree was typically below 5% at low crease penetration depths, but was exponentially higher beyond a critical penetration depth. A rule and channel combination with a wider clearance shifted the critical depth to larger values. The creasing severity parameter, termed the creasing draw, converged the cracking degree data from different rule and channel combinations to a single curve. The creasing draw was derived from the same analytical expres-sions as the transverse shear strain and quantifies the length of paper that is drawn into the channel during creasing. The critical draw is defined as the draw at which cracking becomes greater than 5%, which corresponds with the point at which cracking becomes exponential. The critical draw is a material/system parameter that defines the level below which cracking is minimal.