Lattice Defects Present beneath Crack Initiation, Propagation, and Final Fracture Regions on the Same Hydrogen Embrittlement Fracture Surface of Martensitic Steel

Atomic-scale lattice defects beneath various hydrogen embrittlement fracture process regions, i.e., different fracture modes, were compared for martensitic steel. The crack initiation region containing quasi-cleavage (QC) and intergranular (IG) fracture, the crack propagation region mostly consistin...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:ISIJ International 2024/09/15, Vol.64(11), pp.1732-1736
Hauptverfasser: Chiba, Takahiro, Takai, Kenichi
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Atomic-scale lattice defects beneath various hydrogen embrittlement fracture process regions, i.e., different fracture modes, were compared for martensitic steel. The crack initiation region containing quasi-cleavage (QC) and intergranular (IG) fracture, the crack propagation region mostly consisting of IG fracture, and the final fracture region completely composed of microvoid coalescence (MVC) were extracted from the same fracture surface and analyzed by low-temperature thermal desorption spectroscopy (L-TDS). The relative shapes of the L-TDS curves were different at the sampling positions, demonstrating at the atomic-scale that the types and numbers of lattice defects formed vary depending on the fracture process and fracture mode.
ISSN:0915-1559
1347-5460
DOI:10.2355/isijinternational.ISIJINT-2024-147