Corrosion Behavior of Seamless Pipeline C–Mn Steel by On-line Controlled Cooling Technique

In order to obtain the low cost seamless pipe with the same mechanical properties of C–Mn–Mo steel, the application of controlled cooling technology was successfully applied to the C–Mn steel. Seamless pipeline C–Mn steel was prepared by on-line controlled cooling technique and corrosion behavior wa...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:ISIJ International 2018/04/15, Vol.58(4), pp.734-741
Hauptverfasser: Li, Zheng, Wu, Qianlin, Zhang, Zhonghua, Di, Hongshuang
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In order to obtain the low cost seamless pipe with the same mechanical properties of C–Mn–Mo steel, the application of controlled cooling technology was successfully applied to the C–Mn steel. Seamless pipeline C–Mn steel was prepared by on-line controlled cooling technique and corrosion behavior was studied experimentally by a salt spray wet/dry cyclic corrosion test. Seamless pipeline C–Mn–Mo steel by traditional quenching and tempering technique was used for comparison. Corrosion rate of C–Mn steel is higher than that of C–Mn–Mo steel in the whole test time. The rust layer of C–Mn steel contained more defects than that of C–Mn–Mo steel. Controlling cooling technique can significantly improve the strength of reduced-cost C–Mn steel, while the phenomenon can not reproduce for corrosion resistance.
ISSN:0915-1559