Deep Drawability and Recrystallization Texture of Rephosphorized Al-killed High Strength Cold-rolled Steel
The deep drawability and the recrystallization texture of rephosphorized Al-killed high strength steels (P: -0.07%) were studied as compared with those of a conventional Al-killed steel (P: 0.016%). A rephosphorized Al-killed steel shows the peak r-value at a certain heating rate in annealing as wel...
Gespeichert in:
Veröffentlicht in: | Transactions of the Iron and Steel Institute of Japan 1982, Vol.22(9), pp.732-738 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The deep drawability and the recrystallization texture of rephosphorized Al-killed high strength steels (P: -0.07%) were studied as compared with those of a conventional Al-killed steel (P: 0.016%). A rephosphorized Al-killed steel shows the peak r-value at a certain heating rate in annealing as well as a conventional Al-killed steel. However, phosphorus slightly weakens the retardation effect of AlN on recrystallization, which results in a lower r-value and a lower grain elongation ratio. The preferred orientation of a rephosphorized Al-killed steel is {111} though that of a conventional Al-killed steel is {111} . These results are discussed by taking into account the interaction between phosphorus and AIN precipitation behavior. |
---|---|
ISSN: | 0021-1583 1881-1183 |
DOI: | 10.2355/isijinternational1966.22.732 |