Preparation of Boron Fibre Reinforced Aluminium by a Resistance Sintering Process
Boron fibre reinforced aluminium composite was prepared by a resistance sintering process. A mixture of atomized aluminium powder (−150 mesh) and boron fibre (200 μmφ, tensile strength 3200 MPa) was resistance sintered for 1.2∼1.5s. When a composite was made with an appropriate power input so as not...
Gespeichert in:
Veröffentlicht in: | Transactions of the Japan Institute of Metals 1979, Vol.20(2), pp.51-56 |
---|---|
Hauptverfasser: | , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 56 |
---|---|
container_issue | 2 |
container_start_page | 51 |
container_title | Transactions of the Japan Institute of Metals |
container_volume | 20 |
creator | Akechi, K. Hara, Z. |
description | Boron fibre reinforced aluminium composite was prepared by a resistance sintering process. A mixture of atomized aluminium powder (−150 mesh) and boron fibre (200 μmφ, tensile strength 3200 MPa) was resistance sintered for 1.2∼1.5s. When a composite was made with an appropriate power input so as not to melt aluminium matrix excessively, a sound fibre-matrix interface without a heavy reaction layer was formed and the mechanical properties of the obtained composite was excellent (for example, Al-20 vol%B: 500 MPa). |
doi_str_mv | 10.2320/matertrans1960.20.51 |
format | Article |
fullrecord | <record><control><sourceid>jstage_cross</sourceid><recordid>TN_cdi_crossref_primary_10_2320_matertrans1960_20_51</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>article_matertrans1960_20_2_20_2_51_article_char_en</sourcerecordid><originalsourceid>FETCH-LOGICAL-c427t-7b359449312813e61833034450121259419983745374782203852579e68457ec3</originalsourceid><addsrcrecordid>eNptUNtKAzEQDaJgrf6BD_mBrUkmaXYfa7FaKFhvz0saZ2tKN1sm24f-vZFKQfBhLpwzZ4Y5jN1KMVKgxF3reqSeXEyyGmdMjIw8YwOlQRXaCnnOBkIoWWgN-pJdpbQRwghdwoC9LAl3jlwfusi7ht93lJtZWBHyVwyx6cjjJ59s922IYd_y1YG7zKSQehc98rcQ8_EQ13xJnceUrtlF47YJb37rkH3MHt6nT8Xi-XE-nSwKr5XtC7sCU2ldgVSlBBzLEkCA1kZIJVWmZFWVYLXJYUulBJRGGVvhuNTGooch08e9nrqUCJt6R6F1dKilqH9sqf_aUmfEyCybH2Wb_MAaTyJHffBb_EekjsnI04z_clRjhG8vdHEd</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Preparation of Boron Fibre Reinforced Aluminium by a Resistance Sintering Process</title><source>J-STAGE Free</source><creator>Akechi, K. ; Hara, Z.</creator><creatorcontrib>Akechi, K. ; Hara, Z.</creatorcontrib><description>Boron fibre reinforced aluminium composite was prepared by a resistance sintering process. A mixture of atomized aluminium powder (−150 mesh) and boron fibre (200 μmφ, tensile strength 3200 MPa) was resistance sintered for 1.2∼1.5s. When a composite was made with an appropriate power input so as not to melt aluminium matrix excessively, a sound fibre-matrix interface without a heavy reaction layer was formed and the mechanical properties of the obtained composite was excellent (for example, Al-20 vol%B: 500 MPa).</description><identifier>ISSN: 0021-4434</identifier><identifier>EISSN: 2432-4701</identifier><identifier>DOI: 10.2320/matertrans1960.20.51</identifier><language>eng</language><publisher>The Japan Institute of Metals</publisher><ispartof>Transactions of the Japan Institute of Metals, 1979, Vol.20(2), pp.51-56</ispartof><rights>The Japan Institute of Metals</rights><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c427t-7b359449312813e61833034450121259419983745374782203852579e68457ec3</citedby><cites>FETCH-LOGICAL-c427t-7b359449312813e61833034450121259419983745374782203852579e68457ec3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,776,780,1877,4010,27900,27901,27902</link.rule.ids></links><search><creatorcontrib>Akechi, K.</creatorcontrib><creatorcontrib>Hara, Z.</creatorcontrib><title>Preparation of Boron Fibre Reinforced Aluminium by a Resistance Sintering Process</title><title>Transactions of the Japan Institute of Metals</title><addtitle>Trans. JIM</addtitle><description>Boron fibre reinforced aluminium composite was prepared by a resistance sintering process. A mixture of atomized aluminium powder (−150 mesh) and boron fibre (200 μmφ, tensile strength 3200 MPa) was resistance sintered for 1.2∼1.5s. When a composite was made with an appropriate power input so as not to melt aluminium matrix excessively, a sound fibre-matrix interface without a heavy reaction layer was formed and the mechanical properties of the obtained composite was excellent (for example, Al-20 vol%B: 500 MPa).</description><issn>0021-4434</issn><issn>2432-4701</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1979</creationdate><recordtype>article</recordtype><recordid>eNptUNtKAzEQDaJgrf6BD_mBrUkmaXYfa7FaKFhvz0saZ2tKN1sm24f-vZFKQfBhLpwzZ4Y5jN1KMVKgxF3reqSeXEyyGmdMjIw8YwOlQRXaCnnOBkIoWWgN-pJdpbQRwghdwoC9LAl3jlwfusi7ht93lJtZWBHyVwyx6cjjJ59s922IYd_y1YG7zKSQehc98rcQ8_EQ13xJnceUrtlF47YJb37rkH3MHt6nT8Xi-XE-nSwKr5XtC7sCU2ldgVSlBBzLEkCA1kZIJVWmZFWVYLXJYUulBJRGGVvhuNTGooch08e9nrqUCJt6R6F1dKilqH9sqf_aUmfEyCybH2Wb_MAaTyJHffBb_EekjsnI04z_clRjhG8vdHEd</recordid><startdate>1979</startdate><enddate>1979</enddate><creator>Akechi, K.</creator><creator>Hara, Z.</creator><general>The Japan Institute of Metals</general><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>1979</creationdate><title>Preparation of Boron Fibre Reinforced Aluminium by a Resistance Sintering Process</title><author>Akechi, K. ; Hara, Z.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c427t-7b359449312813e61833034450121259419983745374782203852579e68457ec3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>1979</creationdate><toplevel>online_resources</toplevel><creatorcontrib>Akechi, K.</creatorcontrib><creatorcontrib>Hara, Z.</creatorcontrib><collection>CrossRef</collection><jtitle>Transactions of the Japan Institute of Metals</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Akechi, K.</au><au>Hara, Z.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Preparation of Boron Fibre Reinforced Aluminium by a Resistance Sintering Process</atitle><jtitle>Transactions of the Japan Institute of Metals</jtitle><addtitle>Trans. JIM</addtitle><date>1979</date><risdate>1979</risdate><volume>20</volume><issue>2</issue><spage>51</spage><epage>56</epage><pages>51-56</pages><issn>0021-4434</issn><eissn>2432-4701</eissn><abstract>Boron fibre reinforced aluminium composite was prepared by a resistance sintering process. A mixture of atomized aluminium powder (−150 mesh) and boron fibre (200 μmφ, tensile strength 3200 MPa) was resistance sintered for 1.2∼1.5s. When a composite was made with an appropriate power input so as not to melt aluminium matrix excessively, a sound fibre-matrix interface without a heavy reaction layer was formed and the mechanical properties of the obtained composite was excellent (for example, Al-20 vol%B: 500 MPa).</abstract><pub>The Japan Institute of Metals</pub><doi>10.2320/matertrans1960.20.51</doi><tpages>6</tpages><oa>free_for_read</oa></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0021-4434 |
ispartof | Transactions of the Japan Institute of Metals, 1979, Vol.20(2), pp.51-56 |
issn | 0021-4434 2432-4701 |
language | eng |
recordid | cdi_crossref_primary_10_2320_matertrans1960_20_51 |
source | J-STAGE Free |
title | Preparation of Boron Fibre Reinforced Aluminium by a Resistance Sintering Process |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-30T16%3A12%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-jstage_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Preparation%20of%20Boron%20Fibre%20Reinforced%20Aluminium%20by%20a%20Resistance%20Sintering%20Process&rft.jtitle=Transactions%20of%20the%20Japan%20Institute%20of%20Metals&rft.au=Akechi,%20K.&rft.date=1979&rft.volume=20&rft.issue=2&rft.spage=51&rft.epage=56&rft.pages=51-56&rft.issn=0021-4434&rft.eissn=2432-4701&rft_id=info:doi/10.2320/matertrans1960.20.51&rft_dat=%3Cjstage_cross%3Earticle_matertrans1960_20_2_20_2_51_article_char_en%3C/jstage_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |