Preparation of Boron Fibre Reinforced Aluminium by a Resistance Sintering Process

Boron fibre reinforced aluminium composite was prepared by a resistance sintering process. A mixture of atomized aluminium powder (−150 mesh) and boron fibre (200 μmφ, tensile strength 3200 MPa) was resistance sintered for 1.2∼1.5s. When a composite was made with an appropriate power input so as not...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Transactions of the Japan Institute of Metals 1979, Vol.20(2), pp.51-56
Hauptverfasser: Akechi, K., Hara, Z.
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Boron fibre reinforced aluminium composite was prepared by a resistance sintering process. A mixture of atomized aluminium powder (−150 mesh) and boron fibre (200 μmφ, tensile strength 3200 MPa) was resistance sintered for 1.2∼1.5s. When a composite was made with an appropriate power input so as not to melt aluminium matrix excessively, a sound fibre-matrix interface without a heavy reaction layer was formed and the mechanical properties of the obtained composite was excellent (for example, Al-20 vol%B: 500 MPa).