Solid-state high-oxygen-fugacity processing of BSCCO-2212 superconductors

Silver-sheathed powder-in-tube processed tapes and thick films of the Bi/sub 2/Sr/sub 2/Ca/sub 1/Cu/sub 2/O/sub 8/spl plusmn//spl delta//-type (Bi-2212) superconductor have been annealed under high temperature, high oxygen fugacity (i.e.fO/sub 2/>0.1 MPa) conditions. At sufficiently high temperat...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:IEEE transactions on applied superconductivity 1997-06, Vol.7 (2), p.1533-1536
Hauptverfasser: Gannon, J.J., Sandhage, K.H.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Silver-sheathed powder-in-tube processed tapes and thick films of the Bi/sub 2/Sr/sub 2/Ca/sub 1/Cu/sub 2/O/sub 8/spl plusmn//spl delta//-type (Bi-2212) superconductor have been annealed under high temperature, high oxygen fugacity (i.e.fO/sub 2/>0.1 MPa) conditions. At sufficiently high temperatures and oxygen fugacities, the Bi-2212 phase decomposes into a mixture of solid oxides: a Bi/sub 2/(Sr,Ca)/sub 2/Cu/sub 1/O/sub 8/spl plusmn//spl delta//-type (Bi-2201) phase, an alkaline-earth bismuthate Bi/sub 9/Sr/sub 1/1Ca/sub 5/O/sub y/-type (Bi-91_1_5) phase and CuO. Subsequent reformation of Bi-2212 in pure, flowing oxygen at 0.1 MPa and 860/spl deg/C has yielded plate-like grains with enhanced 00l texture (as discerned from X-ray pole figure analyses and electron microscopy). The values of oxygen fugacity leading to sub-solidus decomposition and reformation of Bi-2212 at 500 to 860/spl deg/C are given. XRD and SEM analyses, as well as preliminary critical current measurements of decomposed and reformed Bi-2212 tapes, are presented.
ISSN:1051-8223
1558-2515