Five high entropy carbide ceramics, (Hf0.2,Nb0.2,Ta0.2,Ti0.2,Zr0.2)C, (Cr0.2,Hf0.2,Ta0.2,Ti0.2,Zr0.2)C, (Hf0.2,Mo0.2,Ta0.2,Ti0.2,Zr0.2)C, (Hf0.2,Ta0.2,Ti0.2,W0.2,Zr0.2)C, and (Hf0.2,Mo0.2,Ti0.2,W0.2,Zr0.2)C, were synthesized by carbothermal reduction of oxides and direct current sintering. The five...
Gespeichert in:
Veröffentlicht in: | Journal of applied physics 2024-04, Vol.135 (16) |
---|---|
Hauptverfasser: | , , , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Five high entropy carbide ceramics, (Hf0.2,Nb0.2,Ta0.2,Ti0.2,Zr0.2)C, (Cr0.2,Hf0.2,Ta0.2,Ti0.2,Zr0.2)C, (Hf0.2,Mo0.2,Ta0.2,Ti0.2,Zr0.2)C, (Hf0.2,Ta0.2,Ti0.2,W0.2,Zr0.2)C, and (Hf0.2,Mo0.2,Ti0.2,W0.2,Zr0.2)C, were synthesized by carbothermal reduction of oxides and direct current sintering. The five high entropy carbide ceramics were determined to be nominally phase-pure with relative densities of more than 98.9% and mean grain sizes of less than 5 μm. Average Vickers hardness values ranged from 19.2 ± 0.4 GPa for (Hf0.2,Nb0.2,Ta0.2,Ti0.2,Zr0.2)C at a load of 2 kgf to 43.5 ± 0.4 GPa for (Hf0.2,Mo0.2,Ti0.2,W0.2,Zr0.2)C at a load of 0.05 kgf. Hardness generally increased with increasing the valence electron concentration and strain as measured by the Williamson–Hall analysis. However, neither correlation was conclusive enough to be a clear indicator of hardness. Instead, it was determined that a combination of effects that includes the valence electron concentration, lattice strain, and grain size all contribute to the hardness of high entropy carbide ceramics. |
---|---|
ISSN: | 0021-8979 1089-7550 |
DOI: | 10.1063/5.0198141 |