First Magnetocrystalline Anisotropy Constants of Some Iron-Silicon Alloys
First magnetocrystalline anisotropy constants K1∞ of 3.6, 6.7, 8.8, and 12.4 wt% silicon in iron alloys have been measured at 77°K and 297°K by determining the torque exerted on {100} single-crystal disks in uniform magnetic fields. The following results on disordered alloys have been obtained: Comp...
Gespeichert in:
Veröffentlicht in: | Journal of applied physics 1961-05, Vol.32 (5), p.857-859 |
---|---|
Hauptverfasser: | , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | First magnetocrystalline anisotropy constants K1∞ of 3.6, 6.7, 8.8, and 12.4 wt% silicon in iron alloys have been measured at 77°K and 297°K by determining the torque exerted on {100} single-crystal disks in uniform magnetic fields. The following results on disordered alloys have been obtained: Composition (wt%Si)Temperature (∘K)K1∞×103(erg cm−3)3.677430±10297360±106.777290±10297205±108.877245±10297165±1012.477120±529778±5
The measurements of this investigation are compared with the previously known studies. The agreement, where an overlap occurs, is satisfactory. |
---|---|
ISSN: | 0021-8979 1089-7550 |