Ferromagnetic resonance of NiCoFe 2 O 4 nanoparticles and microwave absorption properties of flexible NiCoFe 2 O 4 -carbon black/poly(vinyl alcohol) composites

The effect of cationic disorder and particle morphology on the ferromagnetic resonance (FMR) of NiCoFe O nanoparticles (NPs) and the electromagnetic shielding effectiveness of flexible composites (wherein the nanoparticles are used as fillers) has been presented. Upon annealing at 1000 °C, spherical...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Physical chemistry chemical physics : PCCP 2017-08, Vol.19 (31), p.20699-20712
Hauptverfasser: Datt, Gopal, Kotabage, Chetan, Abhyankar, A C
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The effect of cationic disorder and particle morphology on the ferromagnetic resonance (FMR) of NiCoFe O nanoparticles (NPs) and the electromagnetic shielding effectiveness of flexible composites (wherein the nanoparticles are used as fillers) has been presented. Upon annealing at 1000 °C, spherical, ∼25 nm, single crystalline (as-prepared) NPs are transformed into octahedral, ∼200 nm, polycrystalline (annealed) NPs and change the cationic distribution significantly. The effect of shape, size and cationic distribution on the resonance properties has been discussed using the randomly-oriented anisotropic-axis model. The temperature dependent evolution of FMR spectra has been found to be consistent with a Bloch spin-relaxation model. Analysis of the FMR spectra reveals that NiCoFe O nanoparticles have a large internal magnetic field along with broad FMR linewidths of ∼2-3 kOe, signifying high magnetic losses that are essential for the absorption of electromagnetic (EM) waves. Next, NiCoFe O -carbon black (NCF-CB) hybrids grafted in a PVA matrix, as flexible composite films with a thickness of ∼1.5 mm, are assessed for EM wave absorption properties in the range of 8-18 GHz. As compared to annealed-NCF-CB/PVA (21 dB, ∼99.5%), the as-prepared-NCF-CB/PVA composite film exhibits significantly large SE of 27 dB (∼99.9% attenuation of the EM wave), with a dominant contribution from absorption (SE ∼ 21 dB). The electrical conductivity, the electric modulus, and Cole-Cole plots reveal that the dielectric losses in the as-prepared-NCF-CB/PVA have significant contributions from cationic disorder and particle size, as compared to the annealed-NCF-CB/PVA composites. Cationic disorder increases the d-d electron transition probability between adjacent ionic pairs such as Co /Fe and a reduced particle size creates large interfacial polarization in the as-prepared NCF/CB hybrids. Considerably large values of the Landes g-factor, magnetic anisotropy and better impedance matching indicate a dominant magnetic loss contribution in ap-NCF (g = 4.5) as compared to an-NCF (g = 2.5) at 300 K.