Hydrogen-Bonding Properties of Segmented Polyether Poly(urethane urea) Copolymer
FTIR was used to investigate the effects of thermal annealing on the hydrogen-bonding properties of a poly(urethane urea) copolymer. The copolymer was based on ethylene oxide-capped poly(propylene oxide) diol, 4,4‘-diphenylmethane diisocyanate (MDI), and 3,5-diethyltoluenediamine (DETDA). The result...
Gespeichert in:
Veröffentlicht in: | Macromolecules 1997-07, Vol.30 (15), p.4405-4409 |
---|---|
Hauptverfasser: | , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | FTIR was used to investigate the effects of thermal annealing on the hydrogen-bonding properties of a poly(urethane urea) copolymer. The copolymer was based on ethylene oxide-capped poly(propylene oxide) diol, 4,4‘-diphenylmethane diisocyanate (MDI), and 3,5-diethyltoluenediamine (DETDA). The result showed that thermal annealing caused the rise of the number of free urethane groups and the ordering of urea groups. The ordered urea hydrogen bonds were not destroyed below the melting point of the DETDA−MDI hard domain. |
---|---|
ISSN: | 0024-9297 1520-5835 |
DOI: | 10.1021/ma951386e |