Synthesis of Soluble Poly(arylene ether sulfone) Ionomers with Pendant Quaternary Ammonium Groups for Anion Exchange Membranes

A new bisphenol monomer, 2,2′-dimethylaminemethylene-4,4′-biphenol (DABP), was easily prepared by Mannich reaction of dimethylamine and formaldehyde with 4,4′-biphenol. Novel partially fluorinated poly(arylene ether sulfone)s with pendant quaternary ammonium groups were prepared by copolymerization...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Macromolecules 2009-11, Vol.42 (22), p.8711-8717
Hauptverfasser: Wang, Junhua, Zhao, Zhuo, Gong, Feixiang, Li, Shenghai, Zhang, Suobo
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A new bisphenol monomer, 2,2′-dimethylaminemethylene-4,4′-biphenol (DABP), was easily prepared by Mannich reaction of dimethylamine and formaldehyde with 4,4′-biphenol. Novel partially fluorinated poly(arylene ether sulfone)s with pendant quaternary ammonium groups were prepared by copolymerization of DABP, 4,4′-biphenol, and 3,3′,4,4′-tetrafluorodiphenylsulfone, followed by reaction with iodomethane. The resulting copolymers PSQNI-x (where x represents the molar fraction of DABP in the feed) with high molecular weight exhibited outstanding solubility in polar aprotic solvents; thus, the flexible and tough membranes of PSQNI-x with varying ionic content could be prepared by casting from the DMAc solution. Novel anion exchange membranes, PSQNOH-x, were obtained by an anion exchange of PSQNI-x with 1 N NaOH. All PSQNOH-x membranes showed conductivities above 10−2 S cm−1 at room temperature, for example, the hydroxide conductivity of PSQNOH-90 achieved to 8.4 × 10−2 S cm−1, which was thus comparable to the proton conductivity of Nafion 117 (i.e., 9.0 × 10−2 S cm−1).
ISSN:0024-9297
1520-5835
DOI:10.1021/ma901606z