Failure of coatings formed by micro-arc oxidation on titanium under cathodic conditions in H2O2 solution
In the existing chemical stripping methods for micro-arc oxide (MAO) coatings, the application of strong acids (HF, HNO3) or alkali increases the difficulty in post-treatment for stripping solutions. In this study, the failure of MAO coatings on titanium under cathodic conditions was observed in a 6...
Gespeichert in:
Veröffentlicht in: | Surface & coatings technology 2023-09, Vol.468, p.129738, Article 129738 |
---|---|
Hauptverfasser: | , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | In the existing chemical stripping methods for micro-arc oxide (MAO) coatings, the application of strong acids (HF, HNO3) or alkali increases the difficulty in post-treatment for stripping solutions. In this study, the failure of MAO coatings on titanium under cathodic conditions was observed in a 6 % H2O2 solution for the first time. The MAO coatings exfoliated from the TiO2/Ti interface in a visible form within 60 min at a pulsed voltage of 1.6 V (i |
---|---|