The ultrahigh damping capacity of Mg-Sn-Y alloy
High temperature heat treatment Mg-0.69Sn-0.69Y alloy showed a high damping capacity (the damping value is 0.201 at ε=1 × 10−3) and a very low critical strain amplitude at room temperature (εcr1=2.97 × 10−5), which can be attributed to the co-effects of purified matrix phase and interfaces of subgra...
Gespeichert in:
Veröffentlicht in: | Scripta materialia 2023-08, Vol.233, p.115514, Article 115514 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | High temperature heat treatment Mg-0.69Sn-0.69Y alloy showed a high damping capacity (the damping value is 0.201 at ε=1 × 10−3) and a very low critical strain amplitude at room temperature (εcr1=2.97 × 10−5), which can be attributed to the co-effects of purified matrix phase and interfaces of subgrains. The substructure is unstable and the damping capacity decreases with the increasing temperature.
[Display omitted] |
---|---|
ISSN: | 1359-6462 1872-8456 |
DOI: | 10.1016/j.scriptamat.2023.115514 |