Enhanced hot deformation property of Al2O3/Cu–Cr composite fabricated by internal oxidation

The plastic deformability of ODS copper (Al2O3/Cu composite) always limits its widespread commercial application. In this work, the thermodynamically metastable mono-phase CuCr alloy was used to fabricate 2.5 vol%Al2O3/Cu-0.3 vol%Cr by an internal oxidation method with a subsequent solution treatmen...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science & engineering. A, Structural materials : properties, microstructure and processing Structural materials : properties, microstructure and processing, 2024-05, Vol.899, p.146463, Article 146463
Hauptverfasser: Xu, Guoyang, Guo, Xiuhua, Li, Shaolin, Song, Kexing, Song, Hao, Su, Hui
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The plastic deformability of ODS copper (Al2O3/Cu composite) always limits its widespread commercial application. In this work, the thermodynamically metastable mono-phase CuCr alloy was used to fabricate 2.5 vol%Al2O3/Cu-0.3 vol%Cr by an internal oxidation method with a subsequent solution treatment to improve the plastic deformation ability. The influence of dissolved Cr on the hot deformation property and dynamic recrystallization (DRX) behavior of Al2O3/Cu composite was studied, and the softening mechanism of Al2O3/Cu–Cr composite was revealed. The results show that the solid solution of Cr at high temperature can significantly improve the hot deformability of Al2O3/Cu composite. The maximum reduction of peak stress of 2.5 vol%Al2O3/Cu-0.3 vol%Cr composite is 57 % lower than that of 2.8 vol% Al2O3/Cu composite. Furthermore, the DRX critical values of 2.5 vol%Al2O3/Cu-0.3 vol%Cr composite is lower than that of 2.8 vol% Al2O3/Cu composite, and the DRX occurs earlier in Al2O3/Cu–Cr composite. The strain-compensated constructive model of Al2O3/Cu–Cr composite was established with a relation coefficient (R2) of 0.92, which proves the accuracy of the model. Finally, the hot processing map of Al2O3/Cu–Cr composite was constructed based on a dynamic analysis model, and the appropriate hot processing parameter of Al2O3/Cu–Cr composite was obtained with temperature of 1205 K–1223 K and strain rate of 0.022 s−1-0.97 s−1. The results are beneficial to improve hot deformation property of Al2O3/Cu–Cr composite and large sized bulks fabrication.
ISSN:0921-5093
1873-4936
DOI:10.1016/j.msea.2024.146463