Study on high temperature processing of biocompatible Ti-10Ta-10Nb alloys
Specimens of Ti-10Ta-10Nb have become hot forging after being heated to the state of α + β or â-phase. Various temperatures (650, 700, 750, 800, 850°C) and strain rates (0.001, 0.01, 0.1, 1, 10 s −1 ) are used. Based on the flow stress data from temperatures and compressive strain rates, a processin...
Gespeichert in:
Veröffentlicht in: | International journal of precision engineering and manufacturing 2013-06, Vol.14 (6), p.1099-1102 |
---|---|
Hauptverfasser: | , , , , , , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Specimens of Ti-10Ta-10Nb have become hot forging after being heated to the state of α + β or â-phase. Various temperatures (650, 700, 750, 800, 850°C) and strain rates (0.001, 0.01, 0.1, 1, 10 s
−1
) are used. Based on the flow stress data from temperatures and compressive strain rates, a processing map was developed. Processing efficiency is high below about 0.1 s
−1
of strain rates and at almost all the temperatures, but reduced at 0.001 s
−1
and 800°C because of the occurring of Shear band. Processing methods for optimal process are summarized on the basis of experimental findings. Bio-compatibility experiments indicated that Ti-10Ta-10Nb alloy is better than the control, Ti-6Al-4V alloy. |
---|---|