Structure and Hot Corrosion Behavior of an Al-Co-Y Co-deposited Coating on TiAl Alloy
The hot corrosion behavior of Al-Co-Y co-deposited coatings on TiAl alloy was investigated in 25% NaCl + 75% K 2 SO 4 molten salt at 850 °C. Results show that O, S and other corrosive media are preferentially corroded by the α 2 phase of the TiAl matrix, generating corrosion products with poor densi...
Gespeichert in:
Veröffentlicht in: | Journal of materials engineering and performance 2023-06, Vol.32 (11), p.4796-4806 |
---|---|
Hauptverfasser: | , , , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The hot corrosion behavior of Al-Co-Y co-deposited coatings on TiAl alloy was investigated in 25% NaCl + 75% K
2
SO
4
molten salt at 850 °C. Results show that O, S and other corrosive media are preferentially corroded by the
α
2
phase of the TiAl matrix, generating corrosion products with poor density and adhesion, resulting in rapid corrosion. The Al-Co-Y co-deposited coating specimens form a dense Al
2
O
3
film during the hot corrosion incubation, which effectively improves the anti-hot corrosion performance of TiAl alloy. During hot corrosion, the Al
2
O
3
film is dissolved and ruptured under the action of mixed salts, losing its protective properties. |
---|---|