Comparative Study of the Photocatalytic Degradation of the Herbicide 2,4-D Using WO3/TiO2 and Fe2O3/TiO2 as Catalysts

In this study, a comparison of the photocatalytic activity efficiency of the catalysts WO 3 /TiO 2 , Fe 2 O 3 /TiO 2 , and TiO 2 in the degradation of the herbicide 2,4-D and its main by-product (2,4-dichlorophenol, 2,4-DCP), under natural sunlight, visible, and UV light, was carried out. The cataly...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Water, air, and soil pollution air, and soil pollution, 2017-10, Vol.228 (10), Article 379
Hauptverfasser: Macías-Tamez, R., Villanueva-Rodríguez, M., Ramos-Delgado, N. A., Maya-Treviño, L., Hernández-Ramírez, A.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In this study, a comparison of the photocatalytic activity efficiency of the catalysts WO 3 /TiO 2 , Fe 2 O 3 /TiO 2 , and TiO 2 in the degradation of the herbicide 2,4-D and its main by-product (2,4-dichlorophenol, 2,4-DCP), under natural sunlight, visible, and UV light, was carried out. The catalysts were synthesized by the sol-gel method. All the catalysts showed anatase crystalline phase, and they exhibited similar values of band gap, specific surface area, and crystallite size; however, different photocatalytic activity was observed under the different light sources. Complete degradation of 2,4-D and near to 89% of mineralization using WO 3 /TiO 2 and Fe 2 O 3 /TiO 2 was achieved after 150 min under solar light, while using TiO 2 sol-gel, lower degradation rate was obtained. By using artificial light (UV and visible lamp), the degradation and mineralization rates were lower than those obtained under natural sunlight. The produced 2,4-DCP intermediate was completely degraded after 240 min under sunlight only with the modified catalysts.
ISSN:0049-6979
1573-2932
DOI:10.1007/s11270-017-3560-9