Effect of degumming on the tensile properties of silkworm (Bombyx mori) silk fiber

Forcibly reeled silkworm (Bombyx mori) silk was used to study how exposure to a degumming treatment (boiling in distilled water for 30 min) affects tensile properties. Because forcibly reeled and naturally spun fibers exhibit comparable mechanical behavior, the results can be generalized to material...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of applied polymer science 2002-05, Vol.84 (7), p.1431-1437
Hauptverfasser: Pérez-Rigueiro, J., Elices, M., Llorca, J., Viney, C.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Forcibly reeled silkworm (Bombyx mori) silk was used to study how exposure to a degumming treatment (boiling in distilled water for 30 min) affects tensile properties. Because forcibly reeled and naturally spun fibers exhibit comparable mechanical behavior, the results can be generalized to material obtained conventionally from cocoons. The effects of degumming include: a decrease in the initial elastic modulus, a decrease in the stress at the proportional limit (yield strength), a change in the qualitative shape of force‐displacement curves, and significant qualitative and quantitative variability in force‐displacement data from samples subjected to nominally identical degumming histories. Immersion in water at room temperature or heating in air at 100°C for 30 min are both qualitatively equivalent to a 30‐min degumming treatment in boiling water, in terms of the effect on silk tensile properties. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 84: 1431–1437, 2002; DOI 10.1002/app.10366