Influence of ultra-thin TiN thickness(1.4 nm and 2.4 nm) on positive bias temperature instability(PBTI)of high-k/metal gate nMOSFETs with gate-last process

The positive bias temperature instability(PBTI) degradations of high-k/metal gate(HK/MG) n MOSFETs with thin TiN capping layers(1.4 nm and 2.4 nm) are systemically investigated. In this paper, the trap energy distribution in gate stack during PBTI stress is extracted by using ramped recovery stress,...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:中国物理B:英文版 2015 (12), p.499-502
1. Verfasser: 祁路伟 杨红 任尚清 徐烨峰 罗维春 徐昊 王艳蓉 唐波 王文武 闫江 朱慧珑 赵超 陈大鹏 叶甜春
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The positive bias temperature instability(PBTI) degradations of high-k/metal gate(HK/MG) n MOSFETs with thin TiN capping layers(1.4 nm and 2.4 nm) are systemically investigated. In this paper, the trap energy distribution in gate stack during PBTI stress is extracted by using ramped recovery stress, and the temperature dependences of PBTI(90℃,125℃, 160℃) are studied and activation energy(Ea) values(0.13 eV and 0.15 eV) are extracted. Although the equivalent oxide thickness(EOT) values of two TiN thickness values are almost similar(0.85 nm and 0.87 nm), the 2.4-nm TiN one(thicker Ti N capping layer) shows better PBTI reliability(13.41% at 0.9 V, 90℃, 1000 s). This is due to the better interfacial layer/high-k(IL/HK) interface, and HK bulk states exhibited through extracting activation energy and trap energy distribution in the high-k layer.