Effect of structural parameters of Gaussian repaired pit on light intensity distribution inside KH2PO4 crystal

KH2PO4 (KDP) crystal with excellent optical properties is a very important element of inertial confinement fusion (ICF) device. However, KDP crystal surface micro-defects severely reduce the crystal laser damage threshold, affecting the crystal service life. In this paper, Gaussian repaired pit is u...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:中国物理B:英文版 2014-08 (8), p.540-547
1. Verfasser: Xiao Yong Chen Ming-Jun Cheng Jian Liao Wei Wang Hai-Jun Li Ming-Quan
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:KH2PO4 (KDP) crystal with excellent optical properties is a very important element of inertial confinement fusion (ICF) device. However, KDP crystal surface micro-defects severely reduce the crystal laser damage threshold, affecting the crystal service life. In this paper, Gaussian repaired pit is used to replace the crystal surface micro-defects, in order to improve the laser damage resistance of the KDP crystal with surface micro-defects. At first, the physical model of Gaussian repaired pit is built by Fourier model method, and the accuracy of the method is analyzed. It is found that the calculation error can be reduced by increasing the product of the width-period ratio and the truncation constant of the repaired pit. The calculation results about the physical model of Gaussian repaired pit show that the light intensity distribution within the crystal is symmetrical, and there are evidently enhanced light intensity regions in the crystal. Meanwhile, the maximum relative intensity inside the KDP crystal decreases gradually with the increase of the width of the Gaussian repaired pit. Secondly, the Gaussian repaired pits with different widths and the same depth of 20 μm are processed by micro-milling. Their surfaces are very smooth and present the ductile cutting state under the microscope. Finally, the laser damage threshold of the Gaussian repaired pits on the surface of the KDP crystal sample is measured by a 3 ω, 6-ns laser. The results showthat the maximum threshold of the Gaussian repaired pits is 3.12 J/cm2, which is 60% higher than the threshold of initial damage point, and the laser damage threshold increases with the increase of the width of the Gaussian repaired pit.
ISSN:1674-1056
2058-3834
DOI:10.1088/1674-1056/23/8/087702