Growth of Superconducting Whiskers

The(1112)and(2212)amorphous strips ofBi(Pb)-Sr-Ca-Cu oxide were prepared bynon-equilibrium solidification of melt-quenchingmethod.A lot of superconducting whiskers havebeen grown up on the strip at 840-860°C in astream of oxygen for 50-150 h,which are usuallyseveral to 10 odd mm in length,several μm...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:材料科学技术学报:英文版 1990 (4), p.235-238
1. Verfasser: 葛云龙 刘清民 金华 常昕
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The(1112)and(2212)amorphous strips ofBi(Pb)-Sr-Ca-Cu oxide were prepared bynon-equilibrium solidification of melt-quenchingmethod.A lot of superconducting whiskers havebeen grown up on the strip at 840-860°C in astream of oxygen for 50-150 h,which are usuallyseveral to 10 odd mm in length,several μm in thick-ness and more than 10μm in width.These whiskershave very excellent flexibility.
ISSN:1005-0302