Temperature Dependence of Red Long Afterglow from Y2O2S:Eu, Ti, Mg

At low temperature, some long-lasting phosphors could not work well in practical applications. So it is necessary to investigate the temperature dependence of the phosphors. The Y2O2S.Eu, Ti, Mg microcrystalline samples were prepared by solid state reaction method. Phosphors were sintered at 1150 ℃...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of rare earths 2006, Vol.24 (1), p.24-24
1. Verfasser: Zhou Dongfang Shi Chaoshu Qi Zeming Liu Miao Tao Ye Liu Bo Chen Yonghu
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:At low temperature, some long-lasting phosphors could not work well in practical applications. So it is necessary to investigate the temperature dependence of the phosphors. The Y2O2S.Eu, Ti, Mg microcrystalline samples were prepared by solid state reaction method. Phosphors were sintered at 1150 ℃ for 20 min in air, putting in and taking out both at high temperature. The emission spectra and the afterglow spectra as well as the thermoluminescence curve were measured for Y2O2S:Eu,