High-Throughput Atomic Layer Deposition of p-Type SnO Thin Film Transistors Using Tin(II)bis(tert-amyloxide)

Spatial atomic layer deposition (sALD) of p-type SnO is demonstrated using a novel liquid ALD precursor, tin(II)-bis(tert-amyloxide), Sn(TAA) 2, and H 2O as the coreactant in a process which shows an increased deposition rate when compared to conventional temporal ALD. Compared to previously reporte...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Advanced Materials Interfaces 2022-03, Vol.9 (9), Article 2101278
Hauptverfasser: Parish, James D., Dogan, Tamer, Gelinck, Gerwin, Snook, Michael W., Straiton, Andrew J., Kronemeijer, Auke J.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Spatial atomic layer deposition (sALD) of p-type SnO is demonstrated using a novel liquid ALD precursor, tin(II)-bis(tert-amyloxide), Sn(TAA) 2, and H 2O as the coreactant in a process which shows an increased deposition rate when compared to conventional temporal ALD. Compared to previously reported temporal ALD chemistries for the deposition of SnO, deposition rates of up to 19.5 times higher are obtained using Sn(TAA) 2 as a precursor in combination with atmospheric pressure sALD. Growths per cycle of 0.55 and 0.09 Å are measured at deposition temperatures of 100 and 210 °C, respectively. Common-gate thin film transistors (TFTs), fabricated using sALD with Sn(TAA) 2 result in linear mobilities of up to 0.4 cm 2 V –1 s –1 and on/off-current ratios, I On/I Off > 10 2. The combination of enhanced precursor chemistry and improved deposition hardware enables unprecedently high deposition rate ALD of p-type SnO, representing a significant step toward high-throughput p-type TFT fabrication on large area and flexible substrates.