Linear friction welding of Ti-6Al-4V alloy fabricated below β-phase transformation temperature

The interfacial temperature, microstructure and hardness distribution of the linear friction welded Ti-6Al-4V joints obtained at different applied pressures were investigated. The sound Ti-6Al-4V alloy joints were successfully fabricated below the β-phase transformation temperature. The increased pr...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Scripta materialia 2021-01, Vol.191, p.12-16
Hauptverfasser: Choi, Jeong-Won, Aoki, Yasuhiro, Ushioda, Kohsaku, Fujii, Hidetoshi
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 16
container_issue
container_start_page 12
container_title Scripta materialia
container_volume 191
creator Choi, Jeong-Won
Aoki, Yasuhiro
Ushioda, Kohsaku
Fujii, Hidetoshi
description The interfacial temperature, microstructure and hardness distribution of the linear friction welded Ti-6Al-4V joints obtained at different applied pressures were investigated. The sound Ti-6Al-4V alloy joints were successfully fabricated below the β-phase transformation temperature. The increased pressure considerably decreased the welding temperature. The dynamically recrystallized ultra-fined α equiaxed grains of 0.2 μm were formed in the weld center of the joint by applying pressure of 550 MPa. Moreover, the hardness of the weld center was higher than that of the base material without the softened region in thermo-mechanical affected zone, which suggests the improved mechanical properties of the joints. [Display omitted]
doi_str_mv 10.1016/j.scriptamat.2020.09.013
format Article
fullrecord <record><control><sourceid>elsevier_webof</sourceid><recordid>TN_cdi_webofscience_primary_000582135200003CitationCount</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S1359646220306023</els_id><sourcerecordid>S1359646220306023</sourcerecordid><originalsourceid>FETCH-LOGICAL-c368t-f0e2c67c717e055c3b632020a8ca8ed4530c271ac6a252a0d8e76b55ee918d2a3</originalsourceid><addsrcrecordid>eNqNkE1OwzAQRiMEEqVwB-9Rgu3UjrssFX9SJTaFrTVxJuAqjSvbpeq1OAhnwqUVXcJqZvG9TzMvywijBaNM3iyKYLxdRVhCLDjltKDjgrLyJBswVfFcjYQ8TXspxrkcSX6eXYSwoJRKxtkg0zPbI3jSemuidT3ZYNfY_o24lsxtLiddPnol0HVuS1qoUwoiNqTGzm3I12e-eoeAJHroQ-t8umHXEXG5Qg9x7fEyO2uhC3h1mMPs5f5uPn3MZ88PT9PJLDelVDFvKXIjK1OxCqkQpqxluXsGlAGFzUiU1PCKgZHABQfaKKxkLQTimKmGQznM1L7XeBeCx1avvF2C32pG9U6UXuijKL3r1nSsk6gjusHatcFY7A3-4smUUDzp42mj5dTGnx-nbt3HhF7_H03p230ak4gPi14fiMZ6NFE3zv597TdIFJmO</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Linear friction welding of Ti-6Al-4V alloy fabricated below β-phase transformation temperature</title><source>Web of Science - Science Citation Index Expanded - 2021&lt;img src="https://exlibris-pub.s3.amazonaws.com/fromwos-v2.jpg" /&gt;</source><source>Access via ScienceDirect (Elsevier)</source><creator>Choi, Jeong-Won ; Aoki, Yasuhiro ; Ushioda, Kohsaku ; Fujii, Hidetoshi</creator><creatorcontrib>Choi, Jeong-Won ; Aoki, Yasuhiro ; Ushioda, Kohsaku ; Fujii, Hidetoshi</creatorcontrib><description>The interfacial temperature, microstructure and hardness distribution of the linear friction welded Ti-6Al-4V joints obtained at different applied pressures were investigated. The sound Ti-6Al-4V alloy joints were successfully fabricated below the β-phase transformation temperature. The increased pressure considerably decreased the welding temperature. The dynamically recrystallized ultra-fined α equiaxed grains of 0.2 μm were formed in the weld center of the joint by applying pressure of 550 MPa. Moreover, the hardness of the weld center was higher than that of the base material without the softened region in thermo-mechanical affected zone, which suggests the improved mechanical properties of the joints. [Display omitted]</description><identifier>ISSN: 1359-6462</identifier><identifier>EISSN: 1872-8456</identifier><identifier>DOI: 10.1016/j.scriptamat.2020.09.013</identifier><language>eng</language><publisher>OXFORD: Elsevier Ltd</publisher><subject>Interfacial temperature ; Linear friction welding (LFW) ; Materials Science ; Materials Science, Multidisciplinary ; Mechanical properties ; Metallurgy &amp; Metallurgical Engineering ; Microstructure ; Nanoscience &amp; Nanotechnology ; Science &amp; Technology ; Science &amp; Technology - Other Topics ; Technology ; Ti alloys</subject><ispartof>Scripta materialia, 2021-01, Vol.191, p.12-16</ispartof><rights>2020</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>true</woscitedreferencessubscribed><woscitedreferencescount>41</woscitedreferencescount><woscitedreferencesoriginalsourcerecordid>wos000582135200003</woscitedreferencesoriginalsourcerecordid><citedby>FETCH-LOGICAL-c368t-f0e2c67c717e055c3b632020a8ca8ed4530c271ac6a252a0d8e76b55ee918d2a3</citedby><cites>FETCH-LOGICAL-c368t-f0e2c67c717e055c3b632020a8ca8ed4530c271ac6a252a0d8e76b55ee918d2a3</cites><orcidid>0000-0003-4053-8107</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.scriptamat.2020.09.013$$EHTML$$P50$$Gelsevier$$Hfree_for_read</linktohtml><link.rule.ids>315,781,785,3551,27929,27930,39263,46000</link.rule.ids></links><search><creatorcontrib>Choi, Jeong-Won</creatorcontrib><creatorcontrib>Aoki, Yasuhiro</creatorcontrib><creatorcontrib>Ushioda, Kohsaku</creatorcontrib><creatorcontrib>Fujii, Hidetoshi</creatorcontrib><title>Linear friction welding of Ti-6Al-4V alloy fabricated below β-phase transformation temperature</title><title>Scripta materialia</title><addtitle>SCRIPTA MATER</addtitle><description>The interfacial temperature, microstructure and hardness distribution of the linear friction welded Ti-6Al-4V joints obtained at different applied pressures were investigated. The sound Ti-6Al-4V alloy joints were successfully fabricated below the β-phase transformation temperature. The increased pressure considerably decreased the welding temperature. The dynamically recrystallized ultra-fined α equiaxed grains of 0.2 μm were formed in the weld center of the joint by applying pressure of 550 MPa. Moreover, the hardness of the weld center was higher than that of the base material without the softened region in thermo-mechanical affected zone, which suggests the improved mechanical properties of the joints. [Display omitted]</description><subject>Interfacial temperature</subject><subject>Linear friction welding (LFW)</subject><subject>Materials Science</subject><subject>Materials Science, Multidisciplinary</subject><subject>Mechanical properties</subject><subject>Metallurgy &amp; Metallurgical Engineering</subject><subject>Microstructure</subject><subject>Nanoscience &amp; Nanotechnology</subject><subject>Science &amp; Technology</subject><subject>Science &amp; Technology - Other Topics</subject><subject>Technology</subject><subject>Ti alloys</subject><issn>1359-6462</issn><issn>1872-8456</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2021</creationdate><recordtype>article</recordtype><sourceid>HGBXW</sourceid><recordid>eNqNkE1OwzAQRiMEEqVwB-9Rgu3UjrssFX9SJTaFrTVxJuAqjSvbpeq1OAhnwqUVXcJqZvG9TzMvywijBaNM3iyKYLxdRVhCLDjltKDjgrLyJBswVfFcjYQ8TXspxrkcSX6eXYSwoJRKxtkg0zPbI3jSemuidT3ZYNfY_o24lsxtLiddPnol0HVuS1qoUwoiNqTGzm3I12e-eoeAJHroQ-t8umHXEXG5Qg9x7fEyO2uhC3h1mMPs5f5uPn3MZ88PT9PJLDelVDFvKXIjK1OxCqkQpqxluXsGlAGFzUiU1PCKgZHABQfaKKxkLQTimKmGQznM1L7XeBeCx1avvF2C32pG9U6UXuijKL3r1nSsk6gjusHatcFY7A3-4smUUDzp42mj5dTGnx-nbt3HhF7_H03p230ak4gPi14fiMZ6NFE3zv597TdIFJmO</recordid><startdate>20210115</startdate><enddate>20210115</enddate><creator>Choi, Jeong-Won</creator><creator>Aoki, Yasuhiro</creator><creator>Ushioda, Kohsaku</creator><creator>Fujii, Hidetoshi</creator><general>Elsevier Ltd</general><general>Elsevier</general><scope>6I.</scope><scope>AAFTH</scope><scope>BLEPL</scope><scope>DTL</scope><scope>HGBXW</scope><scope>AAYXX</scope><scope>CITATION</scope><orcidid>https://orcid.org/0000-0003-4053-8107</orcidid></search><sort><creationdate>20210115</creationdate><title>Linear friction welding of Ti-6Al-4V alloy fabricated below β-phase transformation temperature</title><author>Choi, Jeong-Won ; Aoki, Yasuhiro ; Ushioda, Kohsaku ; Fujii, Hidetoshi</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c368t-f0e2c67c717e055c3b632020a8ca8ed4530c271ac6a252a0d8e76b55ee918d2a3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2021</creationdate><topic>Interfacial temperature</topic><topic>Linear friction welding (LFW)</topic><topic>Materials Science</topic><topic>Materials Science, Multidisciplinary</topic><topic>Mechanical properties</topic><topic>Metallurgy &amp; Metallurgical Engineering</topic><topic>Microstructure</topic><topic>Nanoscience &amp; Nanotechnology</topic><topic>Science &amp; Technology</topic><topic>Science &amp; Technology - Other Topics</topic><topic>Technology</topic><topic>Ti alloys</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Choi, Jeong-Won</creatorcontrib><creatorcontrib>Aoki, Yasuhiro</creatorcontrib><creatorcontrib>Ushioda, Kohsaku</creatorcontrib><creatorcontrib>Fujii, Hidetoshi</creatorcontrib><collection>ScienceDirect Open Access Titles</collection><collection>Elsevier:ScienceDirect:Open Access</collection><collection>Web of Science Core Collection</collection><collection>Science Citation Index Expanded</collection><collection>Web of Science - Science Citation Index Expanded - 2021</collection><collection>CrossRef</collection><jtitle>Scripta materialia</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Choi, Jeong-Won</au><au>Aoki, Yasuhiro</au><au>Ushioda, Kohsaku</au><au>Fujii, Hidetoshi</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Linear friction welding of Ti-6Al-4V alloy fabricated below β-phase transformation temperature</atitle><jtitle>Scripta materialia</jtitle><stitle>SCRIPTA MATER</stitle><date>2021-01-15</date><risdate>2021</risdate><volume>191</volume><spage>12</spage><epage>16</epage><pages>12-16</pages><issn>1359-6462</issn><eissn>1872-8456</eissn><abstract>The interfacial temperature, microstructure and hardness distribution of the linear friction welded Ti-6Al-4V joints obtained at different applied pressures were investigated. The sound Ti-6Al-4V alloy joints were successfully fabricated below the β-phase transformation temperature. The increased pressure considerably decreased the welding temperature. The dynamically recrystallized ultra-fined α equiaxed grains of 0.2 μm were formed in the weld center of the joint by applying pressure of 550 MPa. Moreover, the hardness of the weld center was higher than that of the base material without the softened region in thermo-mechanical affected zone, which suggests the improved mechanical properties of the joints. [Display omitted]</abstract><cop>OXFORD</cop><pub>Elsevier Ltd</pub><doi>10.1016/j.scriptamat.2020.09.013</doi><tpages>5</tpages><orcidid>https://orcid.org/0000-0003-4053-8107</orcidid><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 1359-6462
ispartof Scripta materialia, 2021-01, Vol.191, p.12-16
issn 1359-6462
1872-8456
language eng
recordid cdi_webofscience_primary_000582135200003CitationCount
source Web of Science - Science Citation Index Expanded - 2021<img src="https://exlibris-pub.s3.amazonaws.com/fromwos-v2.jpg" />; Access via ScienceDirect (Elsevier)
subjects Interfacial temperature
Linear friction welding (LFW)
Materials Science
Materials Science, Multidisciplinary
Mechanical properties
Metallurgy & Metallurgical Engineering
Microstructure
Nanoscience & Nanotechnology
Science & Technology
Science & Technology - Other Topics
Technology
Ti alloys
title Linear friction welding of Ti-6Al-4V alloy fabricated below β-phase transformation temperature
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-14T18%3A50%3A25IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-elsevier_webof&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Linear%20friction%20welding%20of%20Ti-6Al-4V%20alloy%20fabricated%20below%20%CE%B2-phase%20transformation%20temperature&rft.jtitle=Scripta%20materialia&rft.au=Choi,%20Jeong-Won&rft.date=2021-01-15&rft.volume=191&rft.spage=12&rft.epage=16&rft.pages=12-16&rft.issn=1359-6462&rft.eissn=1872-8456&rft_id=info:doi/10.1016/j.scriptamat.2020.09.013&rft_dat=%3Celsevier_webof%3ES1359646220306023%3C/elsevier_webof%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rft_els_id=S1359646220306023&rfr_iscdi=true