Nanosulfonated silica incorporated SPEEK/SPVdF-HFP polymer blend membrane for PEM fuel cell application

Sulfonated silica particles are admixed with sulfonated poly (ether ether ketone) (SPEEK)/sulfonated poly (vinylidene fluoride-co-hexafluoropropylene) (SPVdF-HFP), with various ratios by means of solvent casting. X-ray diffraction (XRD), Fourier-transform infrared spectroscopy (FTIR), scanning elect...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Ionics 2020-07, Vol.26 (7), p.3447-3458
Hauptverfasser: Martina, P., Gayathri, R., Pugalenthi, M. Raja, Cao, Guozhong, Liu, Chaofeng, Prabhu, M. Ramesh
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Sulfonated silica particles are admixed with sulfonated poly (ether ether ketone) (SPEEK)/sulfonated poly (vinylidene fluoride-co-hexafluoropropylene) (SPVdF-HFP), with various ratios by means of solvent casting. X-ray diffraction (XRD), Fourier-transform infrared spectroscopy (FTIR), scanning electron microscope (SEM), atomic force microscopy (AFM), and energy-dispersive X-ray spectroscopy (EDAX) were employed for characterizing the polymer electrolytes. Physicochemical and electrochemical characterizations such as ion exchange capacity, water uptake, swelling ratio, lambda values, temperature-dependent proton conductivity, and performance for prepared polymer composites are also analyzed. From the XRD and FTIR confirms the phase analysis and complex formation of the prepared polymer electrolytes. For 6 wt% S-SiO 2 , incorporated polymer membrane shows the high water uptake (36.5%), swelling ratio (15.9%), and ion exchange capacity (1.70 meq g −1 ) values compared to the respective samples. The highest proton conductivity value obtained for the 6 wt% S-SiO 2 incorporated polymer membrane of 80 wt% SPEEK-20 wt% SPVdF-HFP is 7.9 × 10 −2 S cm −1 . The current density and power density value of 354 mA cm −2 and 110 mW cm −2 with an OCV of 0.95 V at 90 °C under the 100% RH.
ISSN:0947-7047
1862-0760
DOI:10.1007/s11581-020-03478-9